KUNIOSHI, C.T.CORREA, O.V.RAMANATHAN, L.V.2014-07-152014-07-302014-07-152014-07-302006KUNIOSHI, C.T.; CORREA, O.V.; RAMANATHAN, L.V. High temperature oxidation and erosion-oxidation behavior of HVOF sprayed Ni-20Cr, WC-20Cr-7Ni and Crsub(3)csub(2)-Ni-20Cr coatings. <b>Surface Engineering</b>, v. 22, n. 2, p. 121-127, 2006. Disponível em: http://repositorio.ipen.br/handle/123456789/5338.0267-0844http://repositorio.ipen.br/handle/123456789/5338121-127closedAccesserosiontemperature range 0400-1000 koxidationnickelchromiumcoatingstungsten carbidescermetscomposite materialselectric heatingsurfacesroughnessHigh temperature oxidation and erosion-oxidation behavior of HVOF sprayed Ni-20Cr, WC-20Cr-7Ni and Crsub(3)csub(2)-Ni-20Cr coatingsArtigo de periódico222https://orcid.org/0000-0003-4822-8840