Characterization using X-ray diffraction and study of the crystallinity of the thermoplastic starch/poly(butylene adipate-co-terephthalate) blends irradiated by gamma rays
Carregando...
Data
2020
Data de publicação:
Orientador
Título da Revista
ISSN da Revista
Título do Volume
É parte de
É parte de
É parte de
Brazilian Journal of Development
Resumo
The aim of this study was to analyze the changes in the structure and crystallinity of non-irradiated and irradiated thermoplastic starch blends (TPS)/poly (butylene adipate-co-terephthalate) - PBAT and also to evaluate the behavior of castor oil replacing glycerol. In this work, the characterization was performed by using X-ray diffraction (XRD), in which the crystallinity index (IC) of non-irradiated and irradiated blends of TPS/PBAT was calculated, through the software Bruker DIFFRAC.EVA® v4.22. For the plastification of the TPS, glycerol, castor oil and TWEEN® 80 were used to verify their compatibility and establish a comparison among the blends. The samples were prepared by extrusion and irradiated at 25 kGy with gamma rays with a 60Co source. However, the crystallinity indexes of the blends were altered according to the plasticizer used and the use of TWEEN® 80. Thus, it was concluded that replacing glycerol with castor oil is feasible in TPS/PBAT blends.
Como referenciar
CASTRO, DIONE P. de; GARCIA, RAFAEL H.L.; SILVA, LEONARDO G. de A. e. Characterization using X-ray diffraction and study of the crystallinity of the thermoplastic starch/poly(butylene adipate-co-terephthalate) blends irradiated by gamma rays. Brazilian Journal of Development, v. 6, n. 3, p. 9635-9643, 2020. DOI: 10.34117/bjdv6n3-005. Disponível em: http://repositorio.ipen.br/handle/123456789/31453. Acesso em: 17 Mar 2025.
Esta referência é gerada automaticamente de acordo com as normas do estilo IPEN/SP (ABNT NBR 6023) e recomenda-se uma verificação final e ajustes caso necessário.