Oxidation of AISI 304L and 348 stainless steels was investigated in water at 1000 – 1350 °C by TGA, SEM, EDS, and Raman spectroscopy. Linear-Parabolic kinetics and multilayer oxide scales with voids were found for both alloys. Based on the experimental results, AISI 304L presented higher oxidation resistance and higher activation energy. Zircaloy-4 kinetic results were used for validation and performance comparison. In severe accidents conditions, stainless steel might lead to a faster hydrogen production comparing to Zircaloy.

Como referenciar
AVELAR, ALAN M.; GIOVEDI, CLAUDIA; ABE, ALFREDO Y.; MOURAO, MARCELO B. Oxidation of AISI 304L and 348 stainless steels in water at high temperatures. Materials Research, v. 23, n. 6, p. 1-7, 2020. DOI: 10.1590/1980-5373-MR-2020-0373. Disponível em: http://repositorio.ipen.br/handle/123456789/31805. Acesso em: 30 Dec 2025.
Esta referência é gerada automaticamente de acordo com as normas do estilo IPEN/SP (ABNT NBR 6023) e recomenda-se uma verificação final e ajustes caso necessário.

Agência de fomento

Coleções