Effect of heating rate on the shrinkage and microstructure of liquid phase sintered SiC ceramics
Carregando...
Data
Data de publicação
Autores IPEN
Orientador
Título da Revista
ISSN da Revista
Título do Volume
É parte de
É parte de
É parte de
Ceramics International
Resumo
This paper describes a study of shrinkage behavior in the liquid phase sintering of silicon carbide, SiC, using eutectic mixtures of Al2O3+Dy2O3 and Al2O3+Yb2O3 as liquid-forming additives. A volume fraction 10% of these mixtures was added to the SiC and homogenized in an attrition mill. Sintering was performed in a horizontal dilatometer at 1800 °C for 60 min, applying heating rates of 10, 20 and 30 °C/min. The results indicate that these heating rates affected neither shrinkage nor microstructure, from the standpoint of the complete sintering cycle. However, significant differences occurred during the non-isothermal sintering stage, leading to very different shrinkage results as a function of the heating rate. Higher heating rates produced lower shrinkage, and the work of final shrinkage occurred during the isothermal stage.
Como referenciar
RIBEIRO, S.; GENOVA, L.A.; RIBEIRO, G.C.; OLIVEIRA, M.R.; BRESSIANI, A.H.A. Effect of heating rate on the shrinkage and microstructure of liquid phase sintered SiC ceramics. Ceramics International, v. 42, n. 15, p. 17398-17404, 2016. DOI: 10.1016/j.ceramint.2016.08.039. Disponível em: http://repositorio.ipen.br/handle/123456789/27200. Acesso em: 30 Dec 2025.
Esta referência é gerada automaticamente de acordo com as normas do estilo IPEN/SP (ABNT NBR 6023) e recomenda-se uma verificação final e ajustes caso necessário.