Incorporation of galvanic waste (Cr, Ni, Cu, Zn, Pb) in a soda-lime-borosilicate glass
| dc.contributor.author | SILVA, A.C. | pt_BR |
| dc.contributor.author | MELLO-CASTANHO, S. | pt_BR |
| dc.contributor.author | GUITIAN, F. | |
| dc.contributor.author | MONTERO, I. | |
| dc.contributor.author | ESTEBAN-CUBILLO, A. | |
| dc.contributor.author | SOBRADOS, I. | |
| dc.contributor.author | SANZ, J. | |
| dc.contributor.author | MOYA, J.S. | |
| dc.coverage | Internacional | pt_BR |
| dc.date.accessioned | 2014-07-15T13:43:11Z | pt_BR |
| dc.date.accessioned | 2014-07-30T11:49:56Z | |
| dc.date.available | 2014-07-15T13:43:11Z | pt_BR |
| dc.date.available | 2014-07-30T11:49:56Z | |
| dc.date.issued | 2008 | pt_BR |
| dc.description.abstract | In the present investigation, a glassing process for galvanic waste (GW) incorporation with a high chemical stability is presented. Glasses with up to 50 wt% of galvanic solid waste by modifications in the basic composition of soda–lime–borosilicate glasses were prepared. After fusing at temperatures up to 1300°C, the glasses were characterized by inductively coupled plasma, scanning electron microscopy/energy-dispersive X-ray spectroscopy, high-temperature microscopy, transmission and reflected light microscopy, nuclear magnetic resonance, X-ray photoelectron spectroscopy, and X-ray diffraction methods. The chemical stability was evaluated by hydrolytic attack assays. Glasses containing up to 40 wt% of GW with a very high chemical stability, similar to bottle glasses, were obtained. | |
| dc.format.extent | 1300-1305 | pt_BR |
| dc.identifier.citation | SILVA, A.C.; MELLO-CASTANHO, S.; GUITIAN, F.; MONTERO, I.; ESTEBAN-CUBILLO, A.; SOBRADOS, I.; SANZ, J.; MOYA, J.S. Incorporation of galvanic waste (Cr, Ni, Cu, Zn, Pb) in a soda-lime-borosilicate glass. <b>Journal of the American Ceramic Society</b>, v. 91, n. 4, p. 1300-1305, 2008. DOI: <a href="https://dx.doi.org/10.1111/j.1551-2916.2008.02311.x">10.1111/j.1551-2916.2008.02311.x</a>. Disponível em: http://repositorio.ipen.br/handle/123456789/5004. | |
| dc.identifier.doi | 10.1111/j.1551-2916.2008.02311.x | |
| dc.identifier.fasciculo | 4 | pt_BR |
| dc.identifier.issn | 0002-7820 | pt_BR |
| dc.identifier.orcid | https://orcid.org/0000-0002-0155-9100 | |
| dc.identifier.uri | http://repositorio.ipen.br/handle/123456789/5004 | pt_BR |
| dc.identifier.vol | 91 | pt_BR |
| dc.relation.ispartof | Journal of the American Ceramic Society | pt_BR |
| dc.rights | closedAccess | en |
| dc.subject | solid wastes | pt_BR |
| dc.subject | hazardous materials | pt_BR |
| dc.subject | borosilicate glass | pt_BR |
| dc.subject | toxicity | pt_BR |
| dc.title | Incorporation of galvanic waste (Cr, Ni, Cu, Zn, Pb) in a soda-lime-borosilicate glass | pt_BR |
| dc.type | Artigo de periódico | pt_BR |
| dspace.entity.type | Publication | |
| ipen.autor | SONIA REGINA HOMEM DE MELLO CASTANHO | |
| ipen.autor | ANTONIO CARLOS DA SILVA | |
| ipen.codigoautor | 1552 | |
| ipen.codigoautor | 2949 | |
| ipen.contributor.ipenauthor | SONIA REGINA HOMEM DE MELLO CASTANHO | |
| ipen.contributor.ipenauthor | ANTONIO CARLOS DA SILVA | |
| ipen.date.recebimento | 09-04 | pt_BR |
| ipen.identifier.fi | 2.101 | pt_BR |
| ipen.identifier.ipendoc | 13649 | pt_BR |
| ipen.identifier.iwos | WoS | pt_BR |
| ipen.range.fi | 1.500 - 2.999 | |
| ipen.type.genre | Artigo | |
| relation.isAuthorOfPublication | 421edd64-5958-445c-9f93-1e13aabaa72a | |
| relation.isAuthorOfPublication | 839a3a2d-55ca-4376-993c-a8279c5cf017 | |
| relation.isAuthorOfPublication.latestForDiscovery | 839a3a2d-55ca-4376-993c-a8279c5cf017 | |
| sigepi.autor.atividade | SILVA, A.C.:2949:720:S | pt_BR |
| sigepi.autor.atividade | MELLO-CASTANHO, S.:1552:720:N | pt_BR |
Pacote Original
1 - 1 de 1