RAFAEL MORGADO BATISTA

Projetos de Pesquisa
Unidades Organizacionais
Cargo

Resultados de Busca

Agora exibindo 1 - 3 de 3
  • Artigo IPEN-doc 24711
    Analysis of the sintering process in gadolinia-doped ceria by thermodilatometry and correlation with microstructure evolution
    2018 - BATISTA, RAFAEL M.; MUCCILLO, E.N.S.
    The non-isothermal sintering process of cerium dioxide containing gadolinium sesquioxide powders within a wide range of specific surface area was investigated by dilatometry. Linear shrinkage data of powder compacts were recorded under several constant rates of heating. Dilatometry data were analyzed by two methodologies enabling to preview the relative density for any temperature/time profile, and determination of the apparent activation energy for sintering. Correlation of dilatometry results with microstructure evolution was also carried out. Remarkable differences in sintering powders with different specific surface areas were found. The apparent activation energy for sintering increases with decreasing specific surface area and, in most cases, it does not change significantly in the approximately 70-85% range of relative density.
  • Artigo IPEN-doc 22677
    Dilatometry analysis of the sintering process of nanostructured gadolinia-doped ceria
    2016 - BATISTA, R.M.; MUCCILLO, E.N.S.
    The sintering process of compacts of nanostructured gadolinia-doped ceria was investigated by dilatometry and by construction of the master sintering curve. Corrections for the thermal expansion of the experimental setup and mass loss were proposed. The aim of this work was to investigate the sintering evolution of compacts constituted by a powder material with very high specific surface area and to verify the effectiveness of the proposed corrections for generating reliable density data. Validation of the obtained results was accomplished by comparison of corrected data with density values obtained for conventionally sintered compacts. Dilatometry experiments were carried out for 3, 6, 10 and 12 C min-1 heating rates. Good convergence of relative density curves calculated from corrected shrinkage data was obtained. The determined value of the activation energy for sintering of nanostructured gadolinia- doped ceria compacts is 576 kJ mol-1.
  • Artigo IPEN-doc 18469
    Caracterização da céria-gadolínia preparada com pós nanométricos
    2012 - BATISTA, R.M.; MUCCILLO, E.N.S.